This is the temp tower of my wood print experiment Cand even se much difference. It goes from 260 to 190. Below 225 gets really flimsy and above 240 melts. But even 230, the “best” one is really bad, and I’m not talking about retraction. Even the layers that melt are inconsistent.

Also it’s not humidity since the filament was in a filament dryer for.16hours.

edit: The nozzle is 0.8

can someone think of anything else?

  • @roofuskit
    link
    English
    14 months ago

    You can’t both push a bunch of extra material and print faster. Hotends have volumetric limits.