Just pulled these out of the pot and awaiting full cure before I can polish.

I am thinking of doing glittery red high values.

  • WoolyNelsonOP
    link
    fedilink
    arrow-up
    5
    ·
    7 months ago

    Not yet (fresh out of the pot), but i will be polishing out any surface issues before they are used.

    • Komodo Rodeo
      link
      fedilink
      arrow-up
      4
      ·
      7 months ago

      Good stuff, how do you ensure that there’s no gapping/bubbling on the interiors?

      • WoolyNelsonOP
        link
        fedilink
        arrow-up
        7
        ·
        7 months ago

        I use a pressure pot to reduce/prevent bubbles and gaps. For the shells,I fill them about a third, then “smoosh” it over every internal surface with a gloved finger. I find this prevents voids in certain numbers.