An addendum to my previous silly ramblings vis-a-vis this weird pile of metal dust I’ve apparently generated.

User @[email protected] lamented the availability of better pictures, and just after replying to their comment about that (i.e., a hair too late) I had a brainwave and I realized that I did indeed still have this amalgamation in the bin and it was still accessible. Thus against my own better judgement and at great personal risk of life, limb, lens, a great deal of itch, and probably mesothelioma, I boxed the lump up and put it in my photo booth very, very carefully indeed. It’s a little misshapen because as I mentioned earlier I had to bodily rip it off of the carpet.

You dorks really are lucky I like you all so much. And I absolutely am not putting this in the photography community. It’s just too damned silly.

Anyway, get a load of this:

I’m going to venture out on a limb and say that I am probably the premier generator of metal shavings around here, bold claim though this may be. Maybe some of you in the audience are machinists or industrial welders or, I don’t know, shipwrights or something. But suffice it to say I probably make more metal dust in a week than the average bear, and the gods alone know that I’ve produced plenty of it in my life in one way or another.

But I’ve still never seen anything like this.

Here’s a focused stacked patch of the stuff. It’s all the same material, albeit probably lightly dusted with a small amount of cast off abrasive material from my grinding belt, which is par for the course with this sort of thing. That’s what the red triangular thing is in the five o’clock position, there. Otherwise it’s steel, including those blue parts. Those have been heated up sufficiently and then cooled, no doubt with the aid of their high velocity trip through the air as they were fired towards the carpet at the base of my workbench, such that they’ve formed an oxidation layer that produces that color. I’m pretty sure it does so through refraction.

Not nearly as much of this was instantly converted to rust as I’d thought.

That was through my 24mm macro prime.

The above is me throwing caution to the wind entirely and holding my 100mm macro prime as close to this stuff as I dare to, which is about an inch and a half. That’s also a focus stack, and really illustrates what I’ve been rabbiting on about, here. This stuff isn’t dust, per se. It’s made of microscopic fibers. If I didn’t know better, and if you all didn’t know the magnification factor involved here, you’d think that these were chips off of a milling machine or possibly some kind of drilling operation. I’ve never managed to make a grinder produce anything like this in all my years.

Or maybe this happens all the time at particular combinations of speeds and grits and this is all old hat. I’ll be damned if I know.

The knock-on effect of this is that the pile of “dust,” for lack of a better word, is all woven and matted together. See here how it resolutely resists being poked. It’s all spongy and springy; metallic Flubber, only as far as I can tell still within the bounds of the laws of thermodynamics. Not at all coincidentally, it behaves a lot like steel wool.

One wonders if the curious feeling of disquietude evoked by this is the same as those guys who documented the Chernobyl elephant’s foot experienced. Only, you know, theirs was probably much less stupid.

The other thing I probably am around here is the maven of focus bracketing and focus stacking. I say this not only because I do a ton of it for the photos in my other posts, but also in a transparent ploy to make you go look up what “maven” means.

Usually the pictures I take aren’t quite this dense. I noticed old Helicon took quite a while longer than usual to chew on this one.

  • Machinist
    link
    fedilink
    English
    arrow-up
    3
    ·
    1 day ago

    What alloy is it? Guessing it has a lot of chrome in it. That shit don’t cut, it just tears at a microscopic level. You probably know since you mention a respirator, grinding stainless can release some weird shit, including hexavalent chromium. Some SS and super alloys will probably give you dick cancer if you’re exposed enough, even through the skin.

    Also, you’ll get a kick out of this. One night I was doing the surface finishing on titanium airframe landing struts (Ti6Al4V). Using an air powered 90deg die grinder at a slow speed, 2" discs, 80 or 120 grit. I was covered in dust, then I smelled something burning. Look down and my shirts on fire. It was a slow creeping line of embers. Very exciting for a minute, and my bellybutton was out for the rest of the shift.

    • dual_sport_dork 🐧🗡️OPM
      link
      fedilink
      arrow-up
      2
      ·
      22 hours ago

      It’s AEB-L. So yes, 13-13.5% chrome I think.

      Given how much aluminum dust I’ve set on fire over the years for… reasons… I imagine titanium behaves in a pretty similar manner. When that stuff goes, it goes.

      • Machinist
        link
        fedilink
        English
        arrow-up
        2
        ·
        5 hours ago

        I actually had to look up AEB-L as I’d never heard of it. That’s a a strange one. An early stainless instead of a modern. A very plain ‘SS’ alloy. Guessing it would work similar to 17-4 which is a dream to cut. 17-4 is quite crisp, not all smeary.

        I bet you found just the right feed/speed for grinding. Each grain of abrasive is ripping a nice long trough of material. Your belt speed is low enough and your feed is high enough that there is no work hardening. Without the work hardening, the grit is staying sharp.

        Titanium’s burn characteristics are similar to magnesium. A little harder to light. Did a bunch of screw machine work with it early in my career. A good fine chip could be lit with a lighter and it was too bright to safely look at.

        Supposedly titanium is unusal in that it nitridizes just like it oxidizes. In other words, it can ‘burn’ under pure nitrogen.

        I’ve heard you can take an old air cooled VW engine block, build a bonfire under it, and eventually it will turn night into day. High magnesium alloy.

        • dual_sport_dork 🐧🗡️OPM
          link
          fedilink
          arrow-up
          2
          ·
          4 hours ago

          Re: feeds and speeds, that is most likely so. I ran this at 80% speed on my belt grinder as I recall. I don’t have any data sheet, best practice, or even rule of thumb to follow for that so I usually just wing it and gauge how things are going based on the look of the sparks being thrown off the bottom.

          For feeds, well, I’m doing that part by hand. I’ll be interested to see if I can reproduce this running the same belt speed on the next batch. We’ll find out in due course since I have more of this steel left over.

          • Machinist
            link
            fedilink
            English
            arrow-up
            2
            ·
            4 hours ago

            Yah, I been doing machining for a minute. Feed/speed can be scienced but in practice it’s really an art. There are so many variables, including the rigidity of the machine, tool variation, temperature, alloy variation, maybe the phase of the moon. You pulling those kind of chips off a belt sander probably means you got gud, your chi was flowing, and the conditions were right.

            Tuning a good cut for milling in 17-4 and many tool steels is similar. It dry cuts well, so if you’re side milling, you get it cutting in a nice heavy roughing pass. It should throw a rooster tail of chips and you tune it so that the chips come off the tool a light straw and hit the table blue. You can actually see the color change happening in the air.

            I love that shit. It’s beautiful.