Im very new to 3d printing and this is my first time using anything other than pla. So far all of my prints are lifting off the bed at the corners. They start off looking beautiful. No stringing, great adhesion, etc. But after a few layers, they start to come off. Especially on larger prints.

Heres my setup:

  • Ender 3 pro with skr mini e3 v2
  • Creality Ender 3 glass bed upgrade
  • Bed temp: 90C
  • Extruder temp: 240C
  • Nozzle diameter: .4
  • Layer height: .2
  • First layer: .45
  • Speed: 60mm/s
  • Slicer: Silc3r

I realize that asking this question is like asking WebMD to dianose my sniffles, cause it can literally be anything, but Im hoping someone with more experience can give me some pointers on what works for them. Thanks yall!

Update: First of all, thank you all so much for the kick ass suggestions! I really appreciate all of your replies. Since pretty much everyone recommended it, I went ahead and got a textured spring steel PEI plate and holy shit, it didn’t disappoint. Adhesion has been fantastic. I also ended up lowering my bed temp down to 75 from 90 and pushing my hotend temp to 245 for the first layer, then back to 240. I got an enclosure to help keep the plate clean but I also stocked up on some blue dawn dish soap. I still have a little more trial and error with print speed and cooling but I’m literally getting the best prints I’ve ever gotten thanks to all of your suggestions. Yall are awesome and I’m really glad I posted here.

  • @Fubar91
    link
    English
    31 year ago

    I like to drop my cooling fan down to 10% and drop my layer hieght slightly for the first 3-5 layers of the prints for PETG. It tends to like to shift a bunch if cooled too quickly. I also have better results on a textured print surface.