    Dry it well. PLA is not super hydroscopic but over 6 years it will soak up a lot of water.

    • Klajan@lemmy.zip
      link
      fedilink
      English
      arrow-up
      1
      ·
      15 days ago

      Funnily I have a similar PLA (maybe 8 years old), it’s very brittle, but if I can get it loaded it print’s fine, though a bit stringy.

      I doubt it’s moisture though, I had in a filament dryer for 2 days and it still behaved the same.

      • roofuskit
        link
        fedilink
        English
        arrow-up
        1
        ·
        15 days ago

        Brittle and stringy are hallmark signs of wet PLA. If it’s sat for a long time it’s likely very saturated. And some dryers take longer due to the way they are designed.

        • Klajan@lemmy.zip
          link
          fedilink
          English
          arrow-up
          1
          ·
          15 days ago

          Yeah, I know, but I was in a dryer for over 48 hours at 50C , and multiple times afterwards when I was drying other spools and it never got better.

          I think it’s just so old and damaged that that is just how it is now. It’s from the previous owner of my printer and just sat out in the open for 7 or 8 years