This is layer 2 or 3. It will be covered by the next few layers but I feel like it shouldn’t be this fugly. I’m using Cura’s Standard Quality except for temp which is set to 205. The filament is Inland PLA.

  • @[email protected]
    link
    fedilink
    English
    911 months ago

    Does that top surface feel ridged? To me this looks more like an issue with either overextrusion or z offset too low than temperature.

    • nomad
      link
      fedilink
      English
      411 months ago

      I second z offset. Weird that this happens only at a certain regular “column”. Could be hiding an underextruded strand on the level below. In that case your temp might not be stable.