I’ve been getting some problem layers with this filament, especially on flat pieces like this. The first layer is always good, but flat layers (top and bottom) that are not on the bed are not great, like the filament is sagging and not connecting to the lines next to it, regardless of if they are supported or not. This one was a flat layer (completely horizontal) that was fully supported with the zigzag supports from the sovol version of cura.

I know ideally I wouldn’t have totally flat overhangs like this but with the piece I want to print there isn’t really a way around that other than printing multiple flat parts and gluing them together.

I am using a Sovol sv06 and overture PLA. I did not have this issue with the sovol silk silver pla.

I’ve tried leveling my bed again and I think mu z offset is OK because the first layers look good. Currently I’m printing another temp tower and will try some other calibration pieces but any help is appreciated

  • @rambos
    link
    English
    911 months ago

    You are underextruding, but it would also help if you add few more top layers. You have gaps in walls as well. You might be underextruding due to wrong flow (or esteps) or too low temp, but there are other possible reasons as well. Try printing at 105% flow

    • @rambos
      link
      English
      511 months ago

      And one more thing, you said your first layer is always good. It can be good because you have perfect nozzle/bed distance and flow, BUT it can also look good if your distance is wrong and you compensate it with flow. So you might need to increase both flow and distance. You can also change flow for first layer only or change flow after first layer

      • @rambos
        link
        English
        311 months ago

        For calibration you need temp tower and flow tower. You can just print hollow single wall cube with no top/bottom to make it quick print. Keep in mind that PLA especially quality one is quite forgiving so temp tower might look the same at all heights. Meassuring diameter and tuning flow will probably solve your problem

        • @jtskywalkerOP
          link
          English
          211 months ago

          Thank you for the information! I did do a temp tower and the layers do look similar but there seemed to be a sweet spot with less sagging and stringing at 200C so I’m printing there. I have not done a flow tower so I will try that and see if I can get the flow calibrated, and re-do my z-offset and bed leveling stuff.

          I am very new to 3d printing (less than a month) so I’m still trying to figure out all the things I can troubleshoot. This is very helpful!

  • @[email protected]
    link
    fedilink
    English
    6
    edit-2
    11 months ago

    In my experience this is just how 90° overhangs are. It can’t be perfectly flat because if it was it would fuse to the temporary supports. You might be able to get better results with better fillament cooling (or lower fillament tempatures), but afaik some artifact will always be there. So unless I’m mistaken you can’t really “fix” this issue and you are most likely better off designing around it and adding some extra tolerance when you have to use overhangs like this.

    • @modesto_hagney
      link
      English
      611 months ago

      You can change the support top layer settings and mess with if there is top layers and how many there are, then adjust the gap between support top layer and the first layer of the print on top of it until it’s supported correctly and comes away easily.

    • @CarlosCheddar
      link
      English
      311 months ago

      Yeah considering this was basically printing in the air, it looks quite good.

    • @jtskywalkerOP
      link
      English
      111 months ago

      I have thought of that too but I didn’t have this issue with the other filament I used. The 90° overhangs were rough, but they didn’t have lines falling off like with this one.

      If I can’t figure this out I will just re-design the piece to print in two parts and get some 3d gloop or something to stick them together

  • @jtskywalkerOP
    link
    English
    311 months ago

    I watched a few videos on adjusting flow rate and ended up checking my e steps and they were quite a bit off. After fixing that I did a single wall cube to test flow rate and the measurements were right on.

    I printed my test piece again and it is way better. I did slice this one in the regular Cura and not the Solvo version since that’s what I was using to generate the flow tests but I had all the settings pretty much the same.

    Thanks to everyone for the help and suggestions! I will be tweaking my flow and support settings a bit more I’m sure but for now I’m happy with the result

  • MeowdyPardner
    link
    fedilink
    211 months ago

    You might be able to get marginal improvement for overhangs by adjusting support z contact distance, if I’m understanding your problem correctly. I’m usually fiddling a bit with mine, too close and supports are hard to remove. Too far and mine looks close to this.

  • @DrKevorkian
    link
    English
    211 months ago

    I’ve had best results with Cura, trees, support interface on using “grid” with “0.8mm interface thickness” and “75% interface density”, and when printing with 0.2 layer thickness and 0.1 gap between support and model (which then snaps to the 0.2 layer thickness)

    • @jtskywalkerOP
      link
      English
      111 months ago

      I’ve tried tree supports when printing miniatures - I’ll start messing with them for other stuff too. Thanks for the tips. I’ll try those settings

  • @jaschen
    link
    English
    011 months ago

    Looks like you might need to level your bed. That or you need to run temperature test cube. Some filament run better in different temperatures. For me, when I find a brand/color that I works well, I keep using it since I know it’s operating temp.

    • @jtskywalkerOP
      link
      English
      111 months ago

      I did do a temp tower test and found a good temperature. I did try running through the auto bed leveling on the SV06 as well and it didn’t change anything. I have read other methods of bed leveling that are better for the SV06 so I may give those a try too.

      I can definitely see the advantage of sticking with one brand of filament. Being new I kind of assumed PLA is PLA but there has been a noticeable difference between the two that I have tried

      • @jaschen
        link
        English
        111 months ago

        Did you ever fix your issue?

        • @jtskywalkerOP
          link
          English
          111 months ago

          Yes, I put a top level comment with details. The e steps were off causing it to under extrude

            • @jtskywalkerOP
              link
              English
              111 months ago

              Oh that’s odd. The direct link to it is here

              • @[email protected]
                link
                fedilink
                English
                211 months ago

                That is odd because your link shows there are 21 comments on the post while for me I can only see 8 comments.

                • @jtskywalkerOP
                  link
                  English
                  111 months ago

                  I have had some similar issues when posting or interacting with other instances, especially kbin.social

                  I have been unable to vote or comment, and I have had other times when I can’t see comments from the other instances and they can’t see mine.

                  Something similar may be going on here with lemmy.one but I don’t know.

          • @jaschen
            link
            English
            211 months ago

            Fantastic! Glad you fixed it :)