Hex key and mini clamp came in handy for battling a lifting edge

  • @Prismo
    link
    English
    2711 months ago

    This really summarises the passive aggressive level you get to with a 3D printer: “Lift off the bed now you little fucker!”

  • @j4k3M
    link
    English
    411 months ago

    You must have been really close to the end for that to work. I’ve tried many hacks but few really work for me in-situ for more that a dozen layers.

    • @4lanOP
      link
      English
      211 months ago

      There wasn’t much left and nothing that would collide with it. Seemed to work well enough

      I usually use glue stick but just ran out

      • @[email protected]
        link
        fedilink
        English
        211 months ago

        Usually? Like for routine pla prints? I’ve found myself having to do this (man I love magigoo) but the masses say I really shouldn’t have to. Kinda validating if this is actually a thing.

        • @IMALlama
          link
          English
          111 months ago

          If you have corners lifting during big prints it’s nearly always due to a bad first layer or warping. An enclosure, even if it has an open lid since PLA doesn’t really like high enclosure temps, would probably do wonders. But if you have an i3 style printer, enclosures can be kind of a PITA. You could also try a draft shield. Basically tell your slicer to print a skirt that’s the same height as the print itself.

          • @TwanHE
            link
            English
            111 months ago

            Pla can also warp when not cooled enough. Although with a a decent textured Pei sheets you should never have pla adhesion issues honestly

      • @[email protected]
        link
        fedilink
        English
        111 months ago

        Have you tried hairspray? I definitely prefer it as it’s easy to put on and gives nice, even coverage.

        • @4lanOP
          link
          English
          111 months ago

          Not yet, I need to try that

  • @i_simp_4_tedcruz
    link
    English
    311 months ago

    Have they not invented blue painters tape where you’re from?

  • @[email protected]
    link
    fedilink
    English
    3
    edit-2
    11 months ago

    I oddly usually have the other problem, my prints stick too good, the bottom of the print is white (though it is black PLA+) and it sometimes deforms my magnetic mat doohickey while trying to pry it free. Drives me crazy.

    • @4lanOP
      link
      English
      211 months ago

      It’s an LED strip diffuser, this is the mount part

  • @[email protected]
    link
    fedilink
    English
    111 months ago

    I had a huge problem with lifting edges. But since I bought Dimafix Spray all of my issues are gone. I also use brim with increased size to ger near perfect result. I print ABS.

    • @4lanOP
      link
      English
      211 months ago

      I usually use glue stick and never have issues but I just ran out.
      Brims are a good idea for the meantime though

      This is only PlA+ so it should be behaving with a heated bed alone

    • @evidences
      link
      English
      111 months ago

      I’ve only done 3 prints with abs but I used a g10 plate and it worked fabulously. I heard one of the damn prints pop off the plate with a snap when the bed dropped below 60c, that was wild to me.

  • 🇰 🌀 🇱 🇦 🇳 🇦 🇰 ℹ️
    link
    fedilink
    English
    1
    edit-2
    11 months ago

    Ever since it was suggested to rub glue stick over the print bed beforehand, I haven’t had a single issue with raising bits of my prints. Bought a huge school supply case of them like 4 years ago. I’ve used up 2 entire sticks.

  • linuxgator
    link
    fedilink
    English
    111 months ago

    Though skeptical about trying it at first, I’ve found that Aquanet hairspray works amazingly on those creality glass beds. Keeps PLA on, and prevents PETG from bonding.

  • @Prismo
    link
    English
    111 months ago

    I also found a huge difference between filaments. Creality was terrible for me, Reflow is great